OFFCUT JOURNAL · BENCH CARD How to Clamp Wood Without Leaving Dents Put a smooth, broad caul between each clamp jaw and the wood. Center the force on the joint and support the opposite face. Use a dry run to see whether the jaws glide, the cauls rock, or the wood dents before adding glue. WORKED EXAMPLE A 2 × 3-inch pad under a narrow jaw On a small pine box, try two smooth scraps measuring 2 × 3 inches under a pair of narrow metal jaws. Keep the whole face of each pad supported by the box wall. Bring the joint together during a dry rehearsal and remove the pads. If one pad leaves a witness line along its edge, check where it tipped or met an unsupported area. Smooth or reposition that pad first. Look for jaw marks after dry clamping Run the dry clamping sequence, remove the pads, and inspect the face in low-angle light for a jaw-shaped mark. FULL METHOD AND DRAWINGS In the offline site folder, open field-notes/clamp-without-leaving-dents.html. SOURCES USDA Forest Products Laboratory · Wood Handbook https://research.fs.usda.gov/fpl/wood-handbook Titebond · Speed Set wood glue technical sheet https://titebond.com/downloads/literature/glues/FF1242_TB_Speed_Set.pdf WOOD Magazine · Hide a sanded-through spot https://www.woodmagazine.com/woodworking-tips/techniques/finishing/spot-removal1 titebond.com · D4d28015 603f 4dfc a7d9 f684acc71207 https://www.titebond.com/print/product/d4d28015-603f-4dfc-a7d9-f684acc71207